Polymer Property : Puncture Energy = 3.61 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 4.90 J
3.61 ft-lb
ISO 6603-2
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber
PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose..