Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 3.62 J | 2.67 ft-lb | Exxon Mobil Method |
ExxonMobil Exceed™ 1023CA Tough Premium Film Resin
(discontinued **) Exceed 1023CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Puncture Energy | 3.62 J | 2.67 ft-lb | Exxon Mobil Method |
ExxonMobil Exceed™ 1518CA Tough Premium Film Resin
(discontinued **) Exceed 1518CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Puncture Energy | 3.62 J | 2.67 ft-lb | ExxonMobil Method |
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Puncture Energy | 3.62 J | 2.67 ft-lb | ExxonMobil Method |
ExxonMobil LDPE LD 319.92 Low Density Polyethylene Resin Product Description: LD 319.92 resin is an 8.7% vinyl acetate copolymer film resin. Film made from LD 319.92 exhibits superior impact strength and heat sealability.Availability: Latin America, North.. |
|||
Puncture Energy | 3.62 J | 2.67 ft-lb | ExxonMobil |
ExxonMobil NTX™ NTX 101 Super Strength Film Resin NTX 101 is a super strength hexene copolymer LLDPE film resin. Films made from this resin have outstanding toughness properties, especially impact and tear strength, compared to other hexene copoly.. |
|||
Puncture Energy | 3.62 J | 2.67 ft-lb | ExxonMobil Method |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Puncture Energy | 3.62 J | 2.67 ft-lb | Dow Method |
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe.. |
|||
Puncture Energy | 3.62 J | 2.67 ft-lb | ExxonMobil Method |
ExxonMobil Enable™ 20-05CB Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |