Mechanical Properties Metric English Comments
Puncture Energy 3.62 J
2.67 ft-lb
Exxon Mobil Method
ExxonMobil Exceed™ 1023CA Tough Premium Film Resin  (discontinued **)
Exceed 1023CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023CA resin have outstanding tensile, impact strength and puncture. These superi..
Puncture Energy 3.62 J
2.67 ft-lb
Exxon Mobil Method
ExxonMobil Exceed™ 1518CA Tough Premium Film Resin  (discontinued **)
Exceed 1518CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518CA resin have outstanding tensile, impact strength and puncture. These superi..
Puncture Energy 3.62 J
2.67 ft-lb
ExxonMobil Method
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin
Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Puncture Energy 3.62 J
2.67 ft-lb
ExxonMobil Method
ExxonMobil LDPE LD 319.92 Low Density Polyethylene Resin
Product Description: LD 319.92 resin is an 8.7% vinyl acetate copolymer film resin. Film made from LD 319.92 exhibits superior impact strength and heat sealability.Availability: Latin America, North..
Puncture Energy 3.62 J
2.67 ft-lb
ExxonMobil
ExxonMobil NTX™ NTX 101 Super Strength Film Resin
NTX 101 is a super strength hexene copolymer LLDPE film resin. Films made from this resin have outstanding toughness properties, especially impact and tear strength, compared to other hexene copoly..
Puncture Energy 3.62 J
2.67 ft-lb
ExxonMobil Method
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin
Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Puncture Energy 3.62 J
2.67 ft-lb
Dow Method
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe..
Puncture Energy 3.62 J
2.67 ft-lb
ExxonMobil Method
ExxonMobil Enable™ 20-05CB Metallocene Polyethylene Resin
Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Copyright © lookpolymers.com All Rights Reserved