Mechanical Properties Metric English Comments
Puncture Energy 2.50 - 4.80 J

@Temperature -30.0 - -30.0 °C
1.84 - 3.54 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 3.10 J Grade Count:4
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Puncture Energy 2.50 - 4.80 J

@Load <=78.5 kg
1.84 - 3.54 ft-lb

@Load <=173 lb
Average value: 3.10 J Grade Count:4
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Puncture Energy 2.50 J

@Temperature -30.0 °C
1.84 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® DP AKV 30 HR EF 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, good heat-ageing resistance and hydrolysis resistance, good flowability (Easy Flow)
Puncture Energy 2.50 J

@Temperature -30.0 °C
1.84 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® DP AKV 30 HR EF 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, good heat-ageing resistance and hydrolysis resistance, good flowability (Easy Flow)
Puncture Energy 2.50 J

@Temperature -30.0 °C
1.84 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber
PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose..
Puncture Energy 2.50 J

@Temperature -30.0 °C
1.84 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber
PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose..
Puncture Energy 2.50 J
1.84 ft-lb
66N; ASTM D5748
Borealis FT5230 Low Density Polyethylene
FT5230 is a Low Density Polyethylene for Film Extrusion. This grade is developed for the production of packaging film with good optical properties for medium duty film applications. Applications: ..
Puncture Energy 2.50 J
1.84 ft-lb
66N; ASTM D5748
Borealis FT5231 Low Density Polyethylene
FT5231 is a Low Density Polyethylene for blown film. Tubular technology. Contains Antioxidant. This grade is developed for the production of packaging film with good optical properties for medium d..
Puncture Energy 2.50 J
1.84 ft-lb
66N; ASTM D5748
Borealis FT5232 Low Density Polyethylene
FT5232 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes medium slip additive and antioxidant. This grade is developed for the production of packaging film with good op..
Puncture Energy 2.50 J
1.84 ft-lb
66N; ASTM D5748
Borealis FT5236 Low Density Polyethylene
FT5236 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes anti-block, antioxidant and medium slip additives. Applications FT5236 has been developed especially for applic..
Puncture Energy 2.50 J

@Temperature -30.0 °C
1.84 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Pocan® B 3235 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding
Copyright © lookpolymers.com All Rights Reserved