Polymer Property : Puncture Energy = 3.54 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 2.50 - 4.80 J

@Temperature -30.0 - -30.0 °C
1.84 - 3.54 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 3.10 J Grade Count:4
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Puncture Energy 2.50 - 4.80 J

@Load <=78.5 kg
1.84 - 3.54 ft-lb

@Load <=173 lb
Average value: 3.10 J Grade Count:4
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..