Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 1.90 - 2.30 J | 1.40 - 1.70 ft-lb | Average value: 2.22 J Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |