Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 1.90 - 2.30 J | 1.40 - 1.70 ft-lb | Average value: 2.22 J Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Puncture Energy | 1.90 J @Temperature -30.0 °C |
1.40 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance |
|||
Puncture Energy | 1.90 J @Temperature -30.0 °C |
1.40 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance |
|||
Puncture Energy | 1.90 J @Temperature -30.0 °C |
1.40 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance |
|||
Puncture Energy | 1.90 J @Temperature -30.0 °C |
1.40 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance |
|||
Puncture Energy | 1.90 J | 1.40 ft-lb | ISO 6603-2 |
Lanxess Pocan® DP BF 4232 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |