Mechanical Properties Metric English Comments
Puncture Energy 1.70 - 2.50 J

@Temperature -30.0 - -30.0 °C
1.25 - 1.84 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 2.10 J Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Puncture Energy 1.70 - 1.70 J

@Temperature -30.0 - -30.0 °C
1.25 - 1.25 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 1.70 J Grade Count:1
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Puncture Energy 1.70 J

@Temperature -30.0 °C
1.25 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BCF 30 X H2.0 901510 Nylon 6, 30% Glass + Carbon Fiber
PA 6, injection molding grade, 30% reinforced (glass fibers + carbon fibers), conductive, intrinsic color black, good heat-ageing resistance
Puncture Energy 1.70 J

@Temperature -30.0 °C
1.25 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BCF 30 X H2.0 901510 Nylon 6, 30% Glass + Carbon Fiber
PA 6, injection molding grade, 30% reinforced (glass fibers + carbon fibers), conductive, intrinsic color black, good heat-ageing resistance
Puncture Energy 1.70 J

@Temperature -30.0 °C
1.25 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage
Puncture Energy 1.70 J

@Temperature -30.0 °C
1.25 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage
Puncture Energy 1.70 J

@Temperature -30.0 °C
1.25 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in..
Puncture Energy 1.70 J

@Temperature -30.0 °C
1.25 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in..
Puncture Energy 1.70 J

@Temperature -30.0 °C
1.25 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Pocan® DP BF 4232 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant
Puncture Energy 1.70 J
1.25 ft-lb
ISO 6603-2
Lanxess Durethan® AKV 15 H2.0 901510 Nylon 66, 15% Glass Fiber
PA 66, injection molding grade, 15% glass fibers, good heat-ageing resistance