Mechanical Properties Metric English Comments
Charpy Impact, Unnotched 54.2 J
40.0 ft-lb
1/2 size bar
Kinetics MIM 4605 Low Alloy Steel (As Sintered)
Low alloy steel, carbon, nickel, molybdenum. A multi-purpose, economical material that offers various strength, hardness, and wear resistance properties depending if it is heat treated and the heat ..
Charpy Impact, Unnotched 54.2 J
40.0 ft-lb
CMW® 3950 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc.
Charpy Impact, Unnotched 54.2 J
40.0 ft-lb
PSM Industries PolyAlloys MIM-4605 quench/temper Low Alloy Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..