Material Notes:
Low alloy steel, carbon, nickel, molybdenum. A multi-purpose, economical material that offers various strength, hardness, and wear resistance properties depending if it is heat treated and the heat treat process used. Magnetic. Can be plated or coated for corrosion resistance. Used by a very wide range of industries including, automotive, consumer product, firearms, power hand tools, structural, and applications where good strength, hardness and wear resistance is required. The as-sintered condition offers better elongation, but with lower hardness and strength when compared to a heat treated conditionProperty values reported are typical for Kinetics' MIM products.Metal Injection Molding General Notes: Fine metal powders (generally
Physical Properties Metric English Comments
Density 7.60 g/cc
0.275 lb/in³
Sintered
Mechanical Properties Metric English Comments
Hardness, Rockwell B 87
87
Tensile Strength, Ultimate 579 MPa
84000 psi
Tensile Strength, Yield 324 MPa
47000 psi
Elongation at Break 15 %
15 %
in 1 inch
Reduction of Area 20 %
20 %
Charpy Impact, Unnotched 54.2 J
40.0 ft-lb
1/2 size bar
Component Elements Properties Metric English Comments
Carbon, C 0.40 - 0.60 %
0.40 - 0.60 %
Iron, Fe 95.4 - 97.9 %
95.4 - 97.9 %
by difference
Molybdenum, Mo 0.20 - 0.50 %
0.20 - 0.50 %
Nickel, Ni 1.5 - 2.5 %
1.5 - 2.5 %
Silicon, Si <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Surface Finish 40 Ra
Users viewing this material also viewed the following: