PSM Industries PolyAlloys MIM-4605 quench/temper Low Alloy Steel

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer PSM Industries
Trade Name PolyAlloys
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries PolyAlloys MIM-4605 quench/temper Low Alloy Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of complexity and near full theoretical density by utilizing Metal Injection Molding (MIM).  MIM can economically produce complex shapes beyond the capability of conventional Powdered Metallurgy.Benefits of Metal Injection Molding96-98% of Theoretical DensityExcellent Mechanical PropertiesAvoids Costly Secondary OperationsExcellent Surface FinishesCapable of Extreme 3-D GeometriesHolds Tight TolerancesExtremely Thin Wall Section CapabilitiesInformation Provided by PolyAlloys, a division of PSM Industries
Physical Properties Metric English Comments
Density 7.50 g/cc
0.271 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 48
48
Macro
55
55
Micro
Tensile Strength, Ultimate >= 1480 MPa
>= 215000 psi
1650 MPa
240000 psi
Typical
Tensile Strength, Yield >= 1310 MPa

@Strain 0.200 %
>= 190000 psi

@Strain 0.200 %
1480 MPa

@Strain 0.200 %
215000 psi

@Strain 0.200 %
Elongation at Yield <= 1.0 %
<= 1.0 %
in 1 in.
2.0 %
2.0 %
in 1 in.; Typical
Modulus of Elasticity 203 GPa
29500 ksi
Charpy Impact, Unnotched 54.2 J
40.0 ft-lb