Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.67 GPa | 967 ksi | |
Mitsui AURUM® JCQ3025 Thermoplastic Polyimide Resin, Wear/Friction Grade
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Flexural Modulus | 6.67 GPa @Thickness 6.40 mm |
967 ksi @Thickness 0.252 in |
15mm/min; ASTM D790 |
LG Chemical LUCON CP2100-KA02 PC+CF Description Injection Molding Grade, PC+CF, Electrostatic Dissipation, Low Surface ResistanceApplication: LCD Tray, HDD BracketCAS No. 103598-77-2 and 7440-44-0Information provided by LG Chemical |
|||
Flexural Modulus | 6.67 GPa @Thickness 6.40 mm |
967 ksi @Thickness 0.252 in |
3mm/min; ASTM D790 |
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+GF20%, General PurposeApplication: HMID, SLMP B, HolderCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 6.67 GPa @Thickness 3.20 mm |
967 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID SG4389B PA66+GF/MF38% Feature: Injection Molding, PA66+GF/MF38%Application: Automotive (Fan & Shroud)CAS No. 32131-17-2, 25038-54-4, 65997-17-3 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Modulus | 6.67 GPa | 967 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN333HB640BL Multi Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 6.67 GPa @Thickness 6.40 mm |
967 ksi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOL GP3400S PP+MF40% Description: Injection Molding, PP+MF40%, General Purpose, Low WarpageApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 12001-26-2Information provided by LG Chemica.. |