Mechanical Properties Metric English Comments
Flexural Modulus 6.57 GPa
953 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® LGK3020 PC (Asia Pacific)
Glass reinforced. Flame retardant.
Flexural Modulus 6.57 GPa

@Thickness 3.20 mm
953 ksi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID GP2151BF PA66+GF15%, Flame Retardant
Feature: Injection Molding, PA66+GF15%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG..
Flexural Modulus 6.57 GPa
953 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP ZFL24 PPE+PS
LNP* LUBRICOMP* ZFL24 is a compound based on PPE+PS resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is: Wear Resistant.
Flexural Modulus 6.57 GPa
953 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Lubricomp ZFL24 PPO
LNP* Lubricomp* ZFL24 is a compound based on Modified Polyphenylene Oxide (PPO) containing glass fiber and PTFE lubricant. Characteristics of this grade are: Internally Lubricated.This data was su..
Flexural Modulus 6.57 GPa
953 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC
LNP* Thermocomp* Lexan_LGK3020 compound is a glass reinforced. Flame retardant.
Flexural Modulus 6.57 GPa
953 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC (Europe-Africa-Middle East)
LNP* Thermocomp* Lexan_LGK3020 compound is a glass reinforced, flame retardant material.
Flexural Modulus 6.57 GPa
953 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C
LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers.
Flexural Modulus 6.57 GPa
953 ksi
ISO 178
Polyplastics Duranex® 3200 Polybutylene Terephthalate (PBT), Standard, 20% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 6.57 GPa
953 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC (Asia Pacific)
Glass reinforced. Flame retardant.