SABIC Innovative Plastics Lexan® LGK3020 PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® LGK3020 PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass reinforced. Flame retardant.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Water Absorption 0.13 %

@Time 86400 sec
0.13 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.00050 - 0.0025 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0025 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0015 - 0.0035 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0035 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 117 MPa
17000 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type I, 50 mm/min; ASTM D638
Flexural Strength 147 MPa
21300 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 6.57 GPa
953 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 27.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 46.8 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 146 °C

@Thickness 6.40 mm
295 °F

@Thickness 0.252 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
UL 94
Electrical Properties Metric English Comments
Dielectric Strength 17.7 kV/mm

@Thickness 3.20 mm
450 kV/in

@Thickness 0.126 in
in oil; ASTM D149