Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.27 GPa | 910 ksi | ASTM D790 |
Quadrant EPP Semitron® 420 ESd V (ASTM Product Data Sheet) |
|||
Flexural Modulus | 6.28 GPa @Thickness 3.20 mm |
910 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2200 PBT+GF20% Description: Injection Molding, PBT+GF20%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Flexural Modulus | 6.28 GPa | 910 ksi | 5 mm/min; ISO 178 |
Gromax BFM30-EL04B2 Nylon 6 30% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 6.28 GPa | 910 ksi | 5 mm/min; ISO 178 |
Gromax BFG15-DN00N1 Nylon 6 16% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 6.27 GPa | 910 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF20 FR 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 6.28 GPa @Thickness 3.20 mm |
910 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LUCON CP6067 PC+CNT+CF Description: Injection Molding, PC+CNT+CF, Electrostatic Dissipation, High Strength, High Flow & Good ProcessabilityApplication: Wafer Carrier Box, Conveyor belt bearing blockCAS No. 103598-77-2, 74.. |