Polymer Property : Flexural Modulus = 6.27 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.27 GPa
910 ksi
ASTM D790
Quadrant EPP Semitron® 420 ESd V (ASTM Product Data Sheet)
Flexural Modulus 6.27 GPa
909 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC
LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added features include: Flame Retardant.
Flexural Modulus 6.27 GPa
909 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC (Asia Pacific)
LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant, Glass Fiber. Added features of this material include: Flame Retardant.
Flexural Modulus 6.27 GPa
909 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF004E PC
LNP THERMOCOMP* DF004E is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 6.27 GPa
909 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP ZF004 PPE+PS
LNP THERMOCOMP* ZF004 is a compound based on PPE+PS resin containing 20% Glass Fiber.
Flexural Modulus 6.27 GPa
909 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF008S PA 66
LNP* THERMOCOMP* RF008S is a compound based on Nylon 6/6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Modulus 6.27 GPa
909 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RX05494 PA 66
LNP* Thermocomp* RX05494 is a compound based on Nylon 6/6 resin containing glass fiber fillers. Added features of this material include: Heat Stabilized.
Flexural Modulus 6.27 GPa
910 ksi
ASTM D790
Techmer ES HiFill FR® PA6/6 GF20 FR 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc.