Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.93 GPa | 860 ksi | ASTM D790 |
Aaron Industries AAROPRENE® GFIPP 2040 High Impact Glass Filled Polypropylene AAROPRENE® GFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Flexural Modulus | 5.93 GPa | 860 ksi | ASTM D790 |
Asahi Kasei Thermofil N5-15FG-1103 15% Glass Fiber Reinforced, Lubricated Information provided by Asahi Thermofil |