Mechanical Properties Metric English Comments
Flexural Modulus 5.93 GPa
860 ksi
ASTM D790
Aaron Industries AAROPRENE® GFIPP 2040 High Impact Glass Filled Polypropylene
AAROPRENE® GFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Flexural Modulus 5.93 GPa
860 ksi
ASTM D790
Asahi Kasei Thermofil N5-15FG-1103 15% Glass Fiber Reinforced, Lubricated
Information provided by Asahi Thermofil