Polymer Property : Flexural Modulus = 767 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.29 GPa
767 ksi
ASTM D790
SABIC Innovative Plastics Lexan® LGN2000 PC (Asia Pacific)
Flexural Modulus 5.29 GPa
767 ksi
ASTM D790
LG Chemical LUPOY GP-5200 General Purpose PC/ABS Alloy, 10% Polymer Alloy, High Strength
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Flexural Modulus 5.29 GPa
767 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000 PC (Asia Pacific)
Flexural Modulus 5.29 GPa
767 ksi
ASTM D790
Ecomass® 1050CO94 Copper Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityCopper Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Technical Polymers
Flexural Modulus 5.29 GPa
767 ksi
ASTM D 790
SABIC Innovative Plastics Valox® VSR4150 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.