Polymer Property : Flexural Modulus = 73.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.503 GPa
73.0 ksi
ASTM D790
ExxonMobil Escorene® LL-8361 LLDPE, Rotational Molding Powder  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-8 type protection, Good flowUses: Consumer items, Potable water tanks, Laundry tubs
Flexural Modulus 0.503 GPa
73.0 ksi
ASTM D790
Multibase Multi-Flamâ„¢ 2602 PP Polypropylene
Features:Flame RetardantHalogenatedBlooming, None Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Flexural Modulus 0.503 GPa

@Temperature -20.0 °C
73.0 ksi

@Temperature -4.00 °F
ASTM D790
DuPont Elvax® 560 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Flexural Modulus 0.503 GPa
73.0 ksi
Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2503 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with excellent rigidity. It h..
Flexural Modulus 0.503 GPa
73.0 ksi
ASTM D790
ExxonMobil Escorene® LL-8302 LMDPE Rotational Molding Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8302 is the base re..
Flexural Modulus 0.503 GPa
73.0 ksi
ASTM D790
ExxonMobil Escorene® LL-8361 LMDPE Rotational Molding Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8361 is fully formu..