Features:Flame RetardantHalogenatedBlooming, None Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
Elongation at Break 990 %
990 %
ASTM D638
Flexural Modulus 0.503 GPa
73.0 ksi
ASTM D790
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-2
V-2
0.125 in