Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.05 GPa | 1020 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Nemcon™ H PK DP110/X5 PEEK Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT.Information provided by Ovation Polymers |
|||
Flexural Modulus | 7.05 GPa | 1020 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Nemcon™ H PK DP110/X5 Polyetheretherketone Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All sa.. |
|||
Flexural Modulus | 7.05 GPa | 1020 ksi | ISO 178 |
Radici Radilon® SRCP3010LK (dry) Nylon 6 Heat stabilized glass-fiber reinforced and mineral reinforcedInformation provided by Radici group. |
|||
Flexural Modulus | 7.05 GPa | 1020 ksi | ISO 178 |
Nilit FRIANYL A63 CV-CU 0550 Nylon 6.6 for injection molding, 5% carbon fiber reinforced, 50% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 7.05 GPa | 1020 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON KE002 ACETAL LNP* STAT-KON* KE002 is a compound based on Acetal resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 7.05 GPa | 1020 ksi | ISO 178 |
Azdel Plus R451-B02 45% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R451-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr.. |
|||
Flexural Modulus | 7.05 GPa @Temperature 120 °C |
1020 ksi @Temperature 248 °F |
ASTM D790 |
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Flexural Modulus | 7.05 GPa | 1020 ksi | ISO 178 |
Polyplastics Duracon® KT-20 Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Wear resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |