Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® SRCP3010LK (dry) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® SRCP3010LK (dry) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat stabilized glass-fiber reinforced and mineral reinforcedInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 95.0 MPa
13800 psi
ISO 527-1/2
Elongation at Break 2.9 %
2.9 %
ISO 527-1/2
Tensile Modulus 8.20 GPa
1190 ksi
ISO 527-1/2
Flexural Strength 145 MPa
21000 psi
ISO 178
Flexural Modulus 7.05 GPa
1020 ksi
ISO 178
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75/2Af
Vicat Softening Point 210 °C
410 °F
ISO 306
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in