Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 621 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.28 GPa
621 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® BFL2015 PC
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
Flexural Modulus 4.28 GPa
621 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
Flexural Modulus 4.28 GPa
621 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® BFL2015 PC (Europe-Africa-Middle East)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
Flexural Modulus 4.28 GPa
621 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color.
Flexural Modulus 4.28 GPa
621 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF002ERH PC
LNP THERMOCOMP* DF002ERH is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Healthcare, Mold Release.
Flexural Modulus 4.28 GPa
621 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF002ERJ PC
LNP THERMOCOMP* DF002ERJ is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Healthcare.
Flexural Modulus 4.28 GPa
621 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DX06408 PC
LNP THERMOCOMP* DX06408 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Flexural Modulus 4.28 GPa
621 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC
LNP* THERMOCOMP* DX06409 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare.
Flexural Modulus 4.28 GPa
621 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP RF002ES PA 66
LNP THERMOCOMP* RF002ES is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Flexural Modulus 4.28 GPa
621 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Stat-kon AD000Z ABS
LNP* Stat-Kon AD000Z is a compound based on ABS resin with carbon powder. Grade characteristics: a statically conductive extrusion grade.This data was supplied by SABIC-IP for the Americas region...
Flexural Modulus 4.28 GPa
621 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF002ER PC
LNP THERMOCOMP* DF002ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding. Mold Release
Flexural Modulus 4.28 GPa
621 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC (Asia Pacific)
LNP* Thermocomp* DX06409 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Copyright © lookpolymers.com All Rights Reserved