Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.25 GPa | 616 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance. |
|||
Flexural Modulus | 4.25 GPa | 616 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C4210HF is a 10% glass reinforced, non-FR PC+ABS grade with high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low sh.. |
|||
Flexural Modulus | 4.25 GPa | 616 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Flexural Modulus | 4.25 GPa | 616 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Flexural Modulus | 4.25 GPa | 616 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Flexural Modulus | 4.25 GPa | 616 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP SH0430AC_BK1D466 PA12 4.3 specific gravity nylon 12, clean compound system |
|||
Flexural Modulus | 4.25 GPa | 616 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6 LNP* STAT-LOY* PF303 is a Nylon 6 base resin containing 15% Glass Fiber. Added features of this grade includes: Antistat. |
|||
Flexural Modulus | 4.25 GPa | 616 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6 LNP* STAT-LOY* PF303 is a Nylon 6 base resin containing 15% Glass Fiber. Added features of this grade includes: Antistat. |
|||
Flexural Modulus | 4.25 GPa | 616 ksi | ISO 178-93 |
Wellman Wellamid® GFT15N050-WBK 15% Glass Fiber Reinforced, Toughened, Weatherable Nylon 66 Description: Glass Fiber Reinforced, Toughened, Weatherable Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 4.25 GPa | 616 ksi | ASTM D790 |
Ravago Manufacturing Americas Echo® RPC20FG BK Polypropylene Homopolymer Available in North America Filler: Glass Fiber Reinforcement, 20% Filler by weight Recycled Content: YesFeatures: Homopolymer Color: Black Form: Pellets Information provided by Ravago |
|||
Flexural Modulus | 4.25 GPa | 616 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® VX4915 ASA+PBT (Europe-Africa-Middle East) 15% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |