Polymer Property : Flexural Modulus = 4.25 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.25 GPa
616 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS
PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance.
Flexural Modulus 4.25 GPa
616 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS (Europe-Africa-Middle East)
CYCOLOY C4210HF is a 10% glass reinforced, non-FR PC+ABS grade with high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low sh..
Flexural Modulus 4.25 GPa
616 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Xenoy® X4870HH PC+PET
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
Flexural Modulus 4.25 GPa
616 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
Flexural Modulus 4.25 GPa
616 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
Flexural Modulus 4.25 GPa
616 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP SH0430AC_BK1D466 PA12
4.3 specific gravity nylon 12, clean compound system
Flexural Modulus 4.25 GPa
616 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6
LNP* STAT-LOY* PF303 is a Nylon 6 base resin containing 15% Glass Fiber. Added features of this grade includes: Antistat.
Flexural Modulus 4.25 GPa
616 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6
LNP* STAT-LOY* PF303 is a Nylon 6 base resin containing 15% Glass Fiber. Added features of this grade includes: Antistat.
Flexural Modulus 4.25 GPa
616 ksi
ISO 178-93
Wellman Wellamid® GFT15N050-WBK 15% Glass Fiber Reinforced, Toughened, Weatherable Nylon 66
Description: Glass Fiber Reinforced, Toughened, Weatherable Nylon 66Information provided by Wellman.
Flexural Modulus 4.25 GPa
616 ksi
ASTM D790
Ravago Manufacturing Americas Echo® RPC20FG BK Polypropylene Homopolymer
Available in North America Filler: Glass Fiber Reinforcement, 20% Filler by weight Recycled Content: YesFeatures: Homopolymer Color: Black Form: Pellets Information provided by Ravago
Flexural Modulus 4.25 GPa
616 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® VX4915 ASA+PBT (Europe-Africa-Middle East)
15% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.