Mechanical Properties Metric English Comments
Flexural Modulus 2.23 - 3.31 GPa
323 - 480 ksi
Average value: 2.68 GPa Grade Count:11
Overview of materials for PVC, Sheet Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Flexural Modulus 1.65 - 3.31 GPa
239 - 480 ksi
Average value: 2.66 GPa Grade Count:41
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..