Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.23 - 3.31 GPa | 323 - 480 ksi | Average value: 2.68 GPa Grade Count:11 |
Overview of materials for PVC, Sheet Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Flexural Modulus | 1.65 - 3.31 GPa | 239 - 480 ksi | Average value: 2.66 GPa Grade Count:41 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |