Polymer Property : Flexural Modulus = 400.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.759 GPa
400.1 ksi
ASTM D790
Lucent Polymers 6-01 Nylon 6, General Purpose, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizedTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 2.759 GPa
400.1 ksi
ASTM D790
Lucent Polymers CPP-140 Polypropylene Homopolymer, 40% Calcium Carbonate Filled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 2.759 GPa
400.1 ksi
ASTM D790
Lucent Polymers PBT-310 Polybutylene Terephthalate, 30% Glass Fiber/Mineral Reinforced, Low Warp
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Flexural Modulus 2.759 GPa
400.1 ksi
ASTM D790
Lucent Polymers PBT-FR310 Polybutylene Terephthalate, Flame Resistant
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.