Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucent Polymers 6-01 Nylon 6, General Purpose, Injection Grade

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Lucent Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers 6-01 Nylon 6, General Purpose, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Add "R" for Added ReleaseAdd "U" for UV StabilizedTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.013 cm/cm

@Thickness 3.17 mm
0.013 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 73.1 MPa
10600 psi
ASTM D638
Elongation at Break >= 25 %
>= 25 %
ASTM D638
Flexural Strength 103.45 MPa
15004 psi
ASTM D790
Flexural Modulus 2.759 GPa
400.1 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.900 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 210 - 225 °C
410 - 437 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Users viewing this material also viewed the following: