Mechanical Properties Metric English Comments
Flexural Modulus 0.0320 GPa
4.64 ksi
two inch span; ASTM D790
3M Dyneon™ THVP 2030GZ Fluorothermoplastic Granules
THVP 2030GZ is a very flexible, transparent fluoroplastic composed of fluorinated monomers. It is ideal for applications that require the good temperature, chemical and flame resistance of a fluorop..