Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0320 GPa | 4.64 ksi | two inch span; ASTM D790 |
3M Dyneon™ THVP 2030GZ Fluorothermoplastic Granules THVP 2030GZ is a very flexible, transparent fluoroplastic composed of fluorinated monomers. It is ideal for applications that require the good temperature, chemical and flame resistance of a fluorop.. |