Polymer Property : Flexural Modulus = 3740 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 25.8 GPa
3740 ksi
ASTM D790
PolyOne Edgetek® SF2-40CF/000 NATURAL Polyphenylene Sulfide (PPS)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..