Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 25.8 GPa | 3740 ksi | ASTM D790 |
PolyOne Edgetek® SF2-40CF/000 NATURAL Polyphenylene Sulfide (PPS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |