Mechanical Properties Metric English Comments
Flexural Modulus 2.57 GPa
373 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Geloy FXTW26SK ASA
Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.57 GPa
373 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Geloy XTWM200 ASA
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.57 GPa
373 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific)
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 2.57 GPa
373 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East)
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 2.57 GPa

@Thickness 3.17 mm
373 ksi

@Thickness 0.125 in
ASTM D790
PTS PCA-2010NH Non-Bromine, Non-Chlorine, Flame Retardant PC/ABS Alloy
This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 2.57 GPa

@Thickness 3.17 mm
373 ksi

@Thickness 0.125 in
ASTM D790
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy
This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 2.57 GPa
373 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Geloy FXTW26SK ASA (Asia Pacific)
Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Asia Pacific region...
Flexural Modulus 2.57 GPa
373 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Geloy FXTW26SK ASA (Europe-Africa-Middle East)
Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Europe-Africa-Middle..
Flexural Modulus 2.57 GPa

@Thickness 3.17 mm
373 ksi

@Thickness 0.125 in
ASTM D790
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy
This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 2.57 GPa
373 ksi
ASTM D790M
DSM Somos® 7120 Epoxy Photopolymer, Green Parts  (discontinued **)
DescriptionDSM Somos® 7120 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u..
Flexural Modulus 2.57 GPa
373 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON AX00756 ABS
LNP STAT-KON* AX00756 is a compound based on ABS resin containing Stainless Steel. Added feature of this material is: Electrically Conductive.
Flexural Modulus 2.57 GPa
373 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Asia Pacific)
LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Flexural Modulus 2.57 GPa
373 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DSL229 PC
LNP* STAT-KON* DSL229 is a compound based on Polycarbonate resin containing 10% PTFE, 10% Stainless Steel. Added features of this material include: Electrically Conductive, Wear Resistant.
Flexural Modulus 2.57 GPa
373 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DSL229 PC (Asia Pacific)
LNP* Stat-kon* DSL229 is a compound based on Polycarbonate resin containing PTFE, Stainless Steel. Added features of this material include: Electrically Conductive, Internally Lubricated.
Flexural Modulus 2.57 GPa
373 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
Flexural Modulus 2.57 GPa
373 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® V2000DM PBT (Europe-Africa-Middle East)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
Flexural Modulus 2.57 GPa
373 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP AX05466H ABS (Asia Pacific)
LNP* THERMOCOMP* AX05466H is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.
Flexural Modulus 2.57 GPa
373 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Noryl LS175 PPE+HIPS
Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del..
Flexural Modulus 2.57 GPa
373 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Noryl LS175 PPE+HIPS (Europe-Africa-Middle East)
Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del..
Flexural Modulus 2.57 GPa
373 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Stat-kon AD000Z ABS
LNP* Stat-Kon AD000Z is a compound based on ABS resin with carbon powder. Grade characteristics: a statically conductive extrusion grade.This data was supplied by SABIC-IP for the Americas region...
Flexural Modulus 2.57 GPa
373 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® V2000DM PBT
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
Flexural Modulus 2.57 GPa
373 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP 9X10401H ABS
LNP* THERMOCOMP* 9X10401H is a compound based on Polyphenylsulfone containing proprietary filler(s). Added feature of this grade is: X-Ray Opaque.
Flexural Modulus 2.57 GPa

@Thickness 3.17 mm
373 ksi

@Thickness 0.125 in
ASTM D790
Mitsubishi Iupital® F10-02 High Viscosity Acetal Copolymer
Information provided by Polymer Technology and Services, LLC (PTS).