SABIC Innovative Plastics LNP STAT-KON DSL229 PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DSL229 PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* STAT-KON* DSL229 is a compound based on Polycarbonate resin containing 10% PTFE, 10% Stainless Steel. Added features of this material include: Electrically Conductive, Wear Resistant.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Time 86400 sec
0.0050 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 46.0 MPa
6670 psi
ASTM D638
Elongation at Break 4.6 %
4.6 %
ASTM D638
Tensile Modulus 2.45 GPa
355 ksi
50 mm/min; ASTM D638
Flexural Strength 75.0 MPa
10900 psi
ASTM D790
Flexural Modulus 2.57 GPa
373 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.93 J/cm
11.1 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 120 °C

@Thickness 3.20 mm
248 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 10 - 1.00e+6 ohm
10 - 1.00e+6 ohm
ASTM D257
10 - 1.00e+6 ohm
10 - 1.00e+6 ohm
ROA; IEC 60093