Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HF380NS ABS, High Flow, General Anti-Static Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HF380XC ABS, High Flow, High Surface Gloss Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres.. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | DIN 53452; ASTM D790 |
Kolon SPESIN® KP211 General Purpose PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Flexural Modulus | 2.45 GPa @Thickness 6.40 mm |
356 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HI5205 PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® GP1000S PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® SV1120M PBT Description: Injection Molding, PBT, General Purpose, High ViscosityApplication: Films & Sheets, Optical Loose TubeCAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY EF5001RFT PC/ABS Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EU Eco-Label compliantApplication: Display housingCAS: 103598-77-2, 9003-56-9 and 125997-21-9Information provided by LG Chemical.. |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR407D ABS Feature: Electric & Electronic HousingApplication: Electric & Electronic HousingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | |
Shinil Chemical SHINSTAT PC Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® AE-2130 PC/PET, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HI-1001B PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1001T PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® SI-3109GL PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HR-8070 MPPE, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NE-1030 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1023P PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® LX-0989EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | ASTM D790 |
Samyang Triloy® 215 PC/ABS alloy Characteristics:Dimensional stabilityHigh heat resistanceGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl .. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | ASTM D790 |
Samyang Trirex® 3025GRU10 Polycarbonate, 10% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | ASTM D790 |
Samyang Trirex® DMH3000S Polycarbonate, High Flow Flame Retardancy PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.DMH3000S is a high flow, flame retardant grade.Applications: LCD TV Front cover, high .. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® T101 PET Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 2.45 GPa @Thickness 6.40 mm |
356 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron HI40H ABS Injection Molding Grade Automotive applications -Medium Impact, Super High Rigidity, PaintableInformation provided by Bhansali |
|||
Flexural Modulus | 2.45 GPa @Thickness 6.40 mm |
356 ksi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | ASTM D790 |
Aaron Industries AAROPRENE® AEPC 5000-1 Engineered Polycarbonate Resin Melt flow index may be specified. |
|||
Flexural Modulus | 2.45 GPa @Thickness 6.40 mm |
356 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | ASTM D790 |
Samyang Trirex® TH3022N Polycarbonate, High Flow Flame Retardancy PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.TH3022N is a high flow, flame retardant grade.Applications: LCD TV, Laptop and Monitor.. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D201 PBT Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 2.45 GPa @Thickness 6.40 mm |
356 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron HI40H ABS Injection Molding Grade Automotive applications -Medium Impact, Super High Rigidity, PaintableInformation provided by Bhansali |