Polymer Property : Flexural Modulus = 325.6 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.245 GPa
325.6 ksi
ASTM D790
Kleerdex Kydex® IM62 Acrylic/PVC injection Molding Compound  (discontinued **)
High impact injection molding compoundApplications: Appliances, office equipment, electrical products, tools, medical equipment, computer equipmentFeatures: IM62 has a Notched Izod impact resistance..