Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.245 GPa | 325.6 ksi | ASTM D790 |
Kleerdex Kydex® IM62 Acrylic/PVC injection Molding Compound
(discontinued **) High impact injection molding compoundApplications: Appliances, office equipment, electrical products, tools, medical equipment, computer equipmentFeatures: IM62 has a Notched Izod impact resistance.. |