Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.81 GPa | 553 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RBL36L PA 66 LNP* LUBRICOMP* RBL36L is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features s of this grade are: Low Extractable, Wear Resistant. |
|||
Flexural Modulus | 3.81 GPa | 553 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RX85514 PA 66 (Asia Pacific) LNP* LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 3.81 GPa | 552 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® BS-70 70% Barium Sulfate Reinforced Polypropylene Polifil® BS series compounds are homopolymer polypropylene resins reinforced with barium sulfate. They possess increased specific gravity, high flex modulus, high deflection temperature, good chemi.. |