Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.11 GPa | 451 ksi | ASTM D790 |
KYDEX® 2200LT Thermoplastic Sheet for Mass Transit Applications Features:Meets flamespread and smoke development requirements listed in 49 CFR 238Excellent formability and fabrication characteristicsAllows for tight tolerance controlsExcellent resistance to graf.. |
|||
Flexural Modulus | 3.11 GPa | 451 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON EX02598C PEI LNP* STAT-KON* EX02598C is a compound based on Polyetherimide containing Proprietary Filler(s). Added features of this material include: Clean Compound System, Electrically Conductive. |
|||
Flexural Modulus | 3.11 GPa | 451 ksi | ASTM D790 |
Teknor Apex Sinpolene TPP1030 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 30% Filler by Weight Uses: Automotive Applications; Housings Forms: Pellets Processing Method: Injection .. |