Teknor Apex Sinpolene TPP1030 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Talc Filler
Manufacturer Teknor Apex Company
Trade Name Sinpolene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinpolene TPP1030 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 30% Filler by Weight Uses: Automotive Applications; Housings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Melt Flow 9.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.0 MPa
5510 psi
ASTM D638
Elongation at Break 26 %
26 %
ASTM D638
Flexural Strength 54.0 MPa
7830 psi
ASTM D790
Flexural Modulus 3.11 GPa
451 ksi
ASTM D790
Izod Impact, Notched 0.251 J/cm

@Temperature 22.8 °C
0.470 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 133 °C
271 °F
Unannealed; ASTM D648
Vicat Softening Point 154 °C
309 °F
Loading 1 (10N); ASTM D1525