M. Holland Company GS410WC Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company GS410WC Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: High Clarity, High FlowUses: Household Goods, LabwareApprovals: FDA 21 CFR 177.1640 Processing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 200 °C
12 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Elongation at Break 2.0 %
2.0 %
Type I, 2 in/min; ASTM D638
Flexural Modulus 3.07 GPa
445 ksi
at 0.05 in/min; ASTM D790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
at 73°F, 0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
Unannealed; ASTM D648
Vicat Softening Point 95.6 °C
204 °F
ASTM D1525
Descriptive Properties Value Comments
Form Pellets