Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.068 GPa | 299.9 ksi | ASTM D790 |
Ineos Nova FX530 Impact Polystyrene Features: Excellent environmental stress crack resistanceExcellent Izod impact strengthUL Classification 94 HBBalanced physical propertiesApplications: ExtrusionThermoformingSelected injection moldi.. |
|||
Flexural Modulus | 2.068 GPa | 299.9 ksi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers DIAMALOY 1012 ABS/PBT Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.068 GPa | 299.9 ksi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers DIAMALOY 530 PC/PBT Alloy, UV Stabilized/Weatherable Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.068 GPa | 299.9 ksi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers DIAMALOY PCPBT 530 PC/PBT Alloy, UV Stabilized/Weatherable Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.068 GPa | 299.9 ksi | ASTM D790 |
Ineos Nova 5620 High Impact Polystyrene
(discontinued **) High heat resistance, Good balance of toughness and rigidityApplications: Food service itemProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.I.. |
|||
Flexural Modulus | 2.068 GPa | 299.9 ksi | ASTM D790 |
Ineos Nova 5530 High Impact Polystyrene
(discontinued **) Good overall balance of properties, Good toughnessApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C.. |