Mechanical Properties Metric English Comments
Flexural Modulus 2.068 GPa
299.9 ksi
ASTM D790
Ineos Nova FX530 Impact Polystyrene
Features: Excellent environmental stress crack resistanceExcellent Izod impact strengthUL Classification 94 HBBalanced physical propertiesApplications: ExtrusionThermoformingSelected injection moldi..
Flexural Modulus 2.068 GPa
299.9 ksi
chs 0.05 in/min; ASTM D790
Diamond Polymers DIAMALOY 1012 ABS/PBT Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 2.068 GPa
299.9 ksi
chs 0.05 in/min; ASTM D790
Diamond Polymers DIAMALOY 530 PC/PBT Alloy, UV Stabilized/Weatherable
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 2.068 GPa
299.9 ksi
chs 0.05 in/min; ASTM D790
Diamond Polymers DIAMALOY PCPBT 530 PC/PBT Alloy, UV Stabilized/Weatherable
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 2.068 GPa
299.9 ksi
ASTM D790
Ineos Nova 5620 High Impact Polystyrene  (discontinued **)
High heat resistance, Good balance of toughness and rigidityApplications: Food service itemProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.I..
Flexural Modulus 2.068 GPa
299.9 ksi
ASTM D790
Ineos Nova 5530 High Impact Polystyrene  (discontinued **)
Good overall balance of properties, Good toughnessApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C..