Mechanical Properties Metric English Comments
Flexural Modulus 17.7 GPa
2560 ksi
Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D790
Fibre Glast 2000 / 2060 System 2000 Epoxy
System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical ..
Flexural Modulus 17.7 GPa
2560 ksi
Shinil Chemical SHINCON PEEK-CF LCD Rack
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b..
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XK-2307 PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2165BM PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2165M PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2165MC PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XK-2307 PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2165BM PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2165M PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2165MC PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa

@Thickness 3.20 mm
2560 ksi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SP 554 Flame Retardant Polystyrene
Characteristics Very good flow properties Good balance of toughness and rigidity Processing Molding Gas assist molding Applications Large size T.V. Cabinets VCR cabinets Electrical boxes, electr..
Copyright © lookpolymers.com All Rights Reserved