Mechanical Properties Metric English Comments
Flexural Modulus 17.7 GPa
2560 ksi
Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D790
Fibre Glast 2000 / 2060 System 2000 Epoxy
System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical ..
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
Solvay Specialty Polymers Kalix® 3850 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 3850 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in..
Flexural Modulus 17.7 GPa
2560 ksi
Shinil Chemical SHINCON PEEK-CF LCD Rack
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b..
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XK-2307 PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2165BM PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2165M PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2165MC PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XK-2307 PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2165BM PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2165M PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2165MC PPS
Information provided by Samsung Cheil Industries.
Flexural Modulus 17.7 GPa

@Thickness 3.20 mm
2560 ksi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SP 554 Flame Retardant Polystyrene
Characteristics Very good flow properties Good balance of toughness and rigidity Processing Molding Gas assist molding Applications Large size T.V. Cabinets VCR cabinets Electrical boxes, electr..
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
SABIC Innovative Plastics LNP Verton OX07411 PPS (Asia Pacific)
LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
SABIC Innovative Plastics LNP Verton UV00A PPA
LNP VERTON* UV00A is a compound based on Polyphthalamide resin containing Long Glass.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
SABIC Innovative Plastics LNP Verton UV00A PPA (Asia Pacific)
LNP VERTON* UV00A is a compound based on Polyphthalamide resin containing Long Glass.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 17.7 GPa
2570 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Verton UV00ASXS PPA (Europe-Africa-Middle East)
LNP* VERTON* UV00ASXS is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 17.7 GPa
2570 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON UX03320 PPA
LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural.
Flexural Modulus 17.7 GPa
2570 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.
Flexural Modulus 17.7 GPa
2570 ksi
ASTM D790
Plenco 1530 Polyester, Briquette, Injection Molded
PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab..
Flexural Modulus 17.7 GPa
2570 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
LNP Verton™ UF-700-10 Polyphthalamide, Long Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
SABIC Innovative Plastics LNP Verton OX07411 PPS
LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.