Material Notes:
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since both materials cost high, there is a need to design the material with cost effectiveness. Also, the current LCD Rack has a concern of sloughing by CF particulates. SHINIL sloves these problems with the CNT composite of polyphenylene sulfide (PPS), polyether sulfone (PES), PEEK, or polyether imide (PEI) by providing the cost effectiveness combined with enhanced mechanical properties. Especially, the wear resistance (coefficient of friction, coefficient of abrasion) of SHINIL CNT composite was much lower than the current PEEK material, which will provide the material for clean/dust free LCD operation environments.Features and BenefitsPermanent electro conductivityImproved mechanical propertiesNo particulates and no sloughingLighter weightRecyclabilityLow abrasion and frictionImproved surfaceCost effectiveInformation Provided by Shinil Chemical Industry Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 245 MPa
35600 psi
Flexural Strength 343.35 MPa
49799 psi
Flexural Modulus 17.7 GPa
2560 ksi
Izod Impact, Notched 0.883 J/cm
1.65 ft-lb/in
Coefficient of Friction, Dynamic 0.166

@Time 3600 sec,
Pressure 1.96 MPa
0.166

@Time 1.00 hour,
Pressure 284 psi
0.2 m/s
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
Electrical Properties Metric English Comments
Volume Resistivity 1e+05
1e+05
Processing Properties Metric English Comments
Processing Temperature 390 °C
734 °F
Descriptive Properties Value Comments
Abrasion Weight (g) 0.0015
Wear Tester 0.2m/s; 20kgf/cm<sup>2</sup>; 1hr
Coefficient of Abrasion (10-3 cm2-sec/kgf-m-hr) 0.1358
Wear Tester 0.2m/s; 20kgf/cm<sup>2</sup>; 1hr