Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.172 - 1.724 GPa | 170.0 - 250.0 ksi | Polypropylene; ASTM D790M |
DSM Somos® 9120 The need for movable parts is a constant when it comes to prototyping. Being able to ensure the proper fit for parts within a component can save both time and money. Somos® 9120 creates semi-transp.. |