Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.172 GPa | 170.0 ksi | ISO METHOD 178 |
NYCOA 2012 Copolymer Nylon easy flowing, exceptional toughness and flexibility with lower water absorptionInformation provided by NYCOA, Inc. |
|||
Flexural Modulus | 1.172 GPa | 170.0 ksi | ASTM D790 |
Chevron Phillips Marlex® HXM 50100-02 Extra high molecular weight hexene copolymer
(discontinued **) Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesCharacteristics:.. |
|||
Flexural Modulus | 1.172 GPa | 170.0 ksi | ASTM D790 |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Flexural Modulus | 1.172 GPa | 170.0 ksi | ASTM D790 |
Eastman Tenite 307E4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Flexural Modulus | 1.172 GPa | 170.0 ksi | ASTM D790 |
Eastman Tenite 380A3V32818 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Flexural Modulus | 1.172 GPa | 170.0 ksi | ASTM D790 |
Eastman Tenite Propionate 307A2R30018 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
Flexural Modulus | 1.172 GPa | 170.0 ksi | ASTM D790 |
Eastman Tenite Propionate 371A2R30012 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
Flexural Modulus | 1.172 GPa | 170.0 ksi | ASTM D790 |
Eastman Tenite Propionate 380A2R30018 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
Flexural Modulus | 1.172 GPa | 170.0 ksi | ASTM D790 |
Chevron Phillips Marlex® HXM 50100 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
Flexural Modulus | 1.172 - 1.724 GPa | 170.0 - 250.0 ksi | Polypropylene; ASTM D790M |
DSM Somos® 9120 The need for movable parts is a constant when it comes to prototyping. Being able to ensure the proper fit for parts within a component can save both time and money. Somos® 9120 creates semi-transp.. |